Back to Ganoksin | FAQ | Contact

[Source] Rose gold filled sheets and wire


#1

I was just at a beading show and saw (and bought) some beautiful rose
gold filled chain and some basic findings. Well, there wasn’t enough
for me to do what I really want to do, I wanted to buy some rose gold
filled wire and rose gold filled sheets, but they didn’t sell that.
So, does anyone know of a company that sells this? Its really pretty
and I want to do more with this than just beading and I need to make
more closures than they had at the show anyway to start off with.

Thanks for any help.
Jaynemarie Crawford


#2

I was just at a beading show and saw (and bought) some beautiful rose
gold filled chain and some basic findings. Well, there wasn’t enough
for me to do what I really want to do, I wanted to buy some rose gold
filled wire and rose gold filled sheets, but they didn’t sell that.
So, does anyone know of a company that sells this? Its really pretty
and I want to do more with this than just beading and I need to make
more closures than they had at the show anyway to start off with.

Thanks for any help.
Jaynemarie Crawford


#3

Did a little google search and found that this place
http://www.gsgold.com

sells red or rose gold sheets from 8g to 30g. Not bad prices either
when you consider the rarity of them. They have it in both 14K and
18K and they also carry the new Green Gold.

Also found Rose gold sheets in 9K to 18K gold at

http://www.pasternakfindings.com

They carry soldering sheets in rose gold too. The come in standard
70mm width and cut to length. I think this place is a little cheaper
than GS Gold.

Hope this helps.
Michele
MikiCat Designs
Web: www.mikicatdesigns.com


#4

I’ve been searching through google and I have not come up with any
store that sells Rose GOLD FILLED Sheets and Wire. I can find stores
that sell Rose gold, but not Gold Filled. Since I’m trying to come
up with a reasonably priced line of gold filled jewelry, I need a
source other than the one that I bought the chain from. They only
sell Pendants and charms and a few lobster claws, so I need some
source of material to make some more original jewelry from their
starting points.

Thank you,
Jaynemarie


#5

Try wire-sculpture.com for the wire


#6

You can find Rose gold-filled wire at these locations:

http://wire-sculpture.com
http://www.pasternakfindings.com
http://www.libertywireartworks.com

There are even suppliers on Artfire.com that are selling rose
gold-filled wire. As for sheets, I believe pasternakfindings.com
sells both gold-filled wire and sheets in rose.

I’m not sure what you googled, but I got a LOT of sources. You just
have to look at them all.

Michele
MikiCat Designs
www.mikicatdesigns.com


#7

I believe these folks claim to have rose gold filled wire. I know
nothing else about them.

http://wire-sculpture.com

Be well Jim J


#8

Hi Michele,

Since I was on vacation and could only get my email sporadically, I
don’t know if I thanked you for your You gave me a great
source; just what I was looking for.

Thank you again,
Jaynemarie