Back to Ganoksin | FAQ | Contact

[Source] 22K or 24K Tube

Does anyone have a source for 1mm or 1.2mm 22K or 24K tubing?

Thanks,
Joel Schwalb
www.schwalbstudio.com

Hoover & Strong has the 22K

Hi Joel.

I don’t know where you can find it,but you can make it by rolling
24k 4.6mm.x.03mm. x 6inches depends how long you need.Start pulling
on the drawplate until it meet, then solder with 18k yellow hard file
extra solder and pull to the desired sized. 24k or 22k are very soft.
Maybe this will help if you can’t find source.

Renato
www.rlrdesigns.com

Hi Joel,

Did you check Hoover & Strong? On p. 172 of their new catalog they
have light wall tubing in 22K starting at 1.0 mm…