Back to Ganoksin | FAQ | Contact

X-acto knife for sheet metal

is there an x-acto knife for sheet metal? i’m using 30 gauge fine silver, could go to 32… i know i can cut it with joyce chens but was thinking something similar to an x acto knife would be easier, it’s intricate-small spaces, etc… tysm