What is the best material to use for the wire used to hang the
jewelry on during plating? It seems that everyone has their own
preference. Is there a standard?

Thank you
jb


#2

Use the recommended by the plating bath chemical company.

Russ Hyder
The Jewelry CAD Institute
www.thejewelrycadinstitute.com


#3

Everyone I’ve ever spoken to says to use gold wire. I use 14k gold
wire to plate rhodium, etc.


#4
Everyone I've ever spoken to says to use gold wire. I use 14k gold
wire to plate rhodium, etc. 

Does the 14K wire discolour, or does it just get plated cleanly