We do make all the wire and plate from granules. I met a jeweller
from the states that was touring the world. He told us that in the
workshop he did his training they had all the wire and plate
supplied you just cut it off as you needed it. I told him not to
tell my jewellers as they will be moving over there. You don’t know
your alive till you have rolled and drawn 2 kilo gold for 1mm wire.
He didn’t like it. But it’s not that bad.
Phil

I agree it is an experience but soooooooo satifisfying… calgang
and I pull to 30ga…It 's a chanllenge to get clear across the