Does anyone know of a wholesale source for fine silver prong
settings? Not sterling silver, which is all I’ve been able to find
so far. I need them for setting such sizes as 3-8 mm round faceted
stones, and a variety of marquise shapes. Thanks!

Julieann


#2

www.artclayworld.com sells a lot of fine silver findings. They are
sold for pushing into clay before firing, but could also be used for
soldering.

Elaine Luther
Chicago area, Illinois, USA
Certified PMC Instructor
@E_Luther


#3

Fine silver prong settings will be a disaster. The material is far
too soft to use as prongs.

Daniel R. Spirer, GG
www.spirersomes.com