I’m new to the group and so far impressed with the quick turn
over on resposes that people have. So Please, be quick it’s the
thirteenth hour on this project and I already late–no one else
probably does this.

I was requested to make a mokume ring for a ring and what I’ve
found is nirtic acid is recomended for etching the surface to
give the diferent colors more distinction. A satin finish
helps, but…

I also have a chunk of iron meteorite(sic?) and once I’ve heated
it up I’m afraid that I’ll ruin the nice texture. But I know the
texture or finish can be re-applied, or etched with nitric acid.

These are my problems and maybe someone out there has a
solution-no pun intended-Thanks Calvin

I was requested to make a mokume ring for a ring and what I’ve
found is nirtic acid is recomended for etching the surface to

Calvin,

Good source for all sorts of chemistry is Bryant Labs, 1101 5th,
Berkeley, CA 94710 Phone 415-526-3141. Only problem is
shipping nitric or most any acid costs an extra fee. I get my
patination chemistry from these folks (one of their specalities).

John

John and Cynthia/MidLife Crisis Enterprises
Maiden Metals/C. T. Designs/ Bloomin’ Wax Works. etc. Don’t be afraid
to go out on a limb…

PO BX 44, Philo, Ca 95466
That’s where the fruit is!