I have been lurking for months now, I find I learn more if I
keep my mouth shut. Please how did you make a vibrator tumbler? I
have been looking at them and think they are over priced. But my
fingers are getting burns and stiff from the buff wheel. mike
@mweller

 Please how did you make a vibrator tumbler? I have been
looking at them and think they are over priced >>

Mike, Many tumblers from jewelry suppliers ARE overpriced, but
tumblers can be found elsewhere. Try Midway- 800-243-3220.
They’re a gun/reloading supplier, but have good tumblers. I have
used several of their tumblers in my manufacturing shop 24 hours
a day, 365 days a year for several years and they have been
great. They also have a lifetime warranty. Metalsmth

I also use 3 vibs from Midway at less than half the cost
elsewhere. They work very, very well. Ron