Amy, I love my copper scrap, full of holes, etc. I usually cut it
smaller and hard-solder it to ring blanks or pin bases of brass or
nickel-silver (nice color contrast). When you patina it (e.g., with
Jax Black) and rub off the excess, you get nice shadows where the
holes are.

Judy Bjorkman