I was starting to archive my blog photographs and just noticed about 5-6 pictures that were not posted in this essay. You will find them under a sub-topic of “WHOOPS!” in the essay named ** “Mini-claw setting” aka => "Pin-setting**". Are these important? YES, these are so very useful for you to see what ‘casting errors’ might sometimes occur!

(I also did some corrections in my grammar and a few techniques.)