Back to Ganoksin | FAQ | Contact

[UK Source] Gilding metal sheet

Does anyone in the UK know where I can get Gilding metal sheet?

Richard
www.richard-whitehouse.co.uk

Richard,

Does anyone in the UK know where I can get Gilding metal sheet? 

I ordered a sheet of 0.9 x 300 x 300mm gilding metal from A J Reeves
some months ago, the cost was around 16. The links are

http://www.ajreeves.com
http://tinyurl.com/yvnrxq

You could also try Aalco on 01753 619 900, although you may find
they only do wholesale.

Finally, try

Model and College Metals, Units 1 & 2, The Cobden Centre, Vere
Street, Salford, M5 2GQ Tel:0161 736 2498, Fax:0161 736 2506

I phoned them, and was asked to “please put your request on fax
since this goes to the bosses’ house”; they have gilding metal in 2’
sheets, 20 gauge, but it has to be ordered in.

Paul Jelley
London

I ordered a sheet of 0.9 x 300 x 300mm gilding metal from A J
Reeves some months ago, the cost was around 16. The links are 

The last time I went hunting for gilding metal (AKA CZ101, CuZn10,
CW501L etc.) I found a place in Theale near Reading who would sell
me some… In 8’x4’ sheets. This was a little more than I needed at
the time.

Peter

I use Edwards Metals Birmingham for guilding metal. They usually
have it in stock and deliver pretty quick.

Keetly Metals, Birmingham is also a pretty wonderfull place,
especially if you can get them to show you around! Old place, big
selection of all sorts of metals, sizes and uses. they sell fine
copper gauze to filter petrol, petrol goes through but water doesn’t
it’s like fine silk fabric, fantastic!

mary