Back to Ganoksin | FAQ | Contact

Two jewelry challenges( anti tarnish)


#1

Hello Sharon, For storage maybe my silverbrite anit tarnish paper
will help. But It is unbelievable that your silver even wants to
tarnish in a sealed bag. I am working on it to export it to the USA. I
can put you on the list to test a piece for free. then you should
give me your address.

I am looking for companies who what to sell this paper for
protecting silver against tarnishing. I a few weeks companies who are
interested can ask for samples and the price list.

Also I am looking for addresses of firm who sell jewellery supplies.

But for now greeting from the Netherlands

Martin Niemeijer