I have what is probably a dumb question, but here goes. When making post earrings from a tube setting, what is the best order and why?
a) Solder back to tube then post to back
b) Solder post to back then back to tube
c) Some other version that I can’t even imagine.

Thanks

Bernie

Option A. Back to tube with hard solder, post to back with medium.

1 Like