Hi there, I’m brand new to epoxy and wondered if anyone can advise me where to find an epoxy that I can customize (color) and that will work with sterling!

Krohn Industries makes a product called Ceramitation which is specifically formulated for jewelry. It is a catalyst hardening resin designed as a replacement for vitreous enamel. The colors come in both translucent and opaque, and can be mixed to make custom hues.

1 Like

I use Alumilite. Mixing colors can be a challenge in small quantities. Look at the Alumilite website and www.resinobsession.com for more information. Good luck…Rob

1 Like

Wow. Thank you so much! I will reach out to them tomorrow. Really appreciate your advice.
Jean M.

Thank you for your direction. appreciate it so much.