Back to Ganoksin | FAQ | Contact

Thin Copper for corrugating

I have ordered from RJ Leahy for years. Their online catalogue can
be found at rjleahy.com. They are located in SF and their online
listing shows 30 and 36 gauge copper. They can get you whatever size
you want - just call!

Donna Blow, dzines by donna

Hi Group,

I buy all my copper from

McMurray Metals
3009 Elm Street
Dallas, Texas 752267047
972-263-

They will ship anywhere. Been in business for about 50 or 60 years in
Dallas.

.016 inch thick Sq foot is $2.25
.021 inch thick Sq foot is $2.80
.027 inch thick Sq foot is $3.50

I buy it all the time for enameling.

Love and God Bless
-randy
http://www.rocksmyth.com