Our teacher used a few drops of liquid dish soap (Dawn, Joy etc.) in
4 oz. Of methyl alcohol. Then put this into a fine mist pump sprayer
for even application. Betsy

A safer alcohol to use, as methyl alcohol is poisonus is high proof
Vodka or if you can get it ethyl alcohol. We use methyl alcohol to
degrease metal and ALWAYS wear gloves and have the exhaust fans
going to remove the fumes.

Mike
Lone Star Technical Service, Your ultrasonic repair guys.