It appears  that C3 is more interested in selling there tester that
product.  Most gemologist have a polariscope that will determine if
the mineral is doubly refractive.  Cheaper testers are sure to
follow.

The double refraction is very obvious. I’d say a good eyeball can
do it :> Carol


| Carol J. Bova @Carol_J_Bova |
| http://www.bovagems.com/ Faceted Emeralds, |
| Tourmalines, Garnets, Aquamarines & more! |
| P.O.Box 5388 Glendale, CA 91221-5388 USA |
| Sponsors of The Eclectic Lapidary e-zine |
| http://www.bovagems.com/eclectic/ |
’’

 The double refraction is very obvious. I'd say a good eyeball can
 do it 

I understand that the doubling is not so obvious through the table
due to the orientation of the crystal in cutting but is obvious
through bezel or crown main facets.