Standard Steam Dewaxer

Does the Standard Steam Dewaxer that I see in the Rio Grande catalog
reduce the time the flask needs to spend in ovens. If so by how much
time?

Andrew McIntyre

I was told I still needed to run the full burn out, so it doesn’t
shorten it. However, it reduces the fumes by something like 90%,
which means I have happier lungs and happier neighbors and less mess
to clean up!

Jeanne