Hi All

For a long time I have been chasing good quality leather cord
between 1.8 to 2mm - in red and they always seem to come off the roll
with kinks in them and do not hang uniformly. Not a good look when
featuring an extra long pendant! Any recommendations would be very
much appreciated! Or even alternative suggestions!

Thanks in advance
Christel van der Laan in West Oz

You could try wetting the leather then hanging it up with a weight on
the end to straighten it while it dries.

HTH
Pat

Christel: Because it was the finest I fond, I have used Greek
leather cord and bought in http://www.btoucan.com