Back to Ganoksin | FAQ | Contact

[Source] Titanium sheet

Hi All

I am looking for Titanium flat sheet, not embossed, in size 3"X3" or
4"X4" in 18 or 20 gauge. No luck on the web.

Shirl Carter

Try McMaster-Carr at http://www.mcmaster.com it is a 6"x 6" sheet but
you can cut it down

Part Number  9051K11
$16.50 Each
Shape Sheets
Sheet Type Plain
Material Grade 2 (40KSI-YS) Titanium
Finish/Coating Unpolished (Mill)
Length 6"
Length Tolerance +1/8"
Width 6"
Width Tolerance +1/8"
Thickness 0.35"
Thickness Tolerance 1.004"
Specifications Met ASTM B265

Standard disclaimer, just a satisfied customer

Jim Binnion

James Binnion Metal Arts
Phone (360) 756-6550
Toll Free (877) 408 7287
=46ax (360) 756-2160


@James_Binnion
Member of the Better Business Bureau

Try Reactive Metals, I have gotten Ti from them before.

Or try McMaster Carr, I know they have a website too and a great
catalog.

Sara
Studio C Designs

Hello Shirl,

I can deliver sheets in titanium no problem, However it will come
from the Netherlands.

Greetings
Martin Niemeijer
N design
compositions in precious metal
Rieteweg 10
8041 AK, Zwolle
Netherlands
info@ndesign.nl; www.ndesign.nl
Phone/fax +31 38 750 1258
mobile +31 6 518 315 76

I have gotten titanium sheet from Sheffield Knifemaker’s Supply in
Florida, 386 775-6453, http://www.sheffieldsupply.com . Their catalog
is downloadable.

Larrie
Corvallis, Oregon

    I have gotten titanium sheet from Sheffield Knifemaker's
Supply in Florida, 386 775-6453, http://www.sheffieldsupply.com .
Their catalog is downloadable. 

It should be noted here that all the titanium products offered by
Sheffields are Grade #5 or 6/4 Titanium. It is 6% Vanadium and 4%
Aluminum. It is very hard! Averaging a Rockwell C=36. It will pretty
much wear the teeth off a jewelers saw. It is used for everything
from jet engine compressor blades to dental implants. It is a poor
blade material. While it is light, it will not hold a sharp edge for
long.

Bill

Reactive Metals Studio, Inc.
PO Box 890 * 600 First North St. * Clarkdale, AZ 86324
Ph-928/634-3434 * Ph-800/876-3434 * Fax-928/634-6734
@Michele_Deborah_Bill

Bill,

I must say thank you for taking the time to inform us of the
properties of the titanium offered by Sheffields. I think it is
important that the properties of various metals be investigated
before just accepting that htey are whatever metal (in this case
titanium) and that they will respond just like the metal you had
purchased before, but in this case att a much lower price. Metal
is not metal.

It should be noted here that all the titanium products offered by
Sheffields are Grade #5 or 6/4 Titanium. It is 6% Vanadium and 4%
Aluminum. It is very hard! Averaging a Rockwell C=36. It will
pretty much wear the teeth off a jewelers saw. It is used for
everything from jet engine compressor blades to dental implants. It
is a poor blade material. While it is light, it will not hold a
sharp edge for long.

Bill