Hello,

Does anyone have a source to buy reticulated silver and gold?

Thank you
Lee Baker

This reads as if you wish to purchase metal already reticulated. Is
that true?

Reactive Metals Studio, Inc.
PO Box 890 * Clarkdale, AZ 86324
Ph-928/634-3434 * Ph-800/876-3434 * Fax-928/634-6734
E-mail- @Michele_Deborah_Bill
Catalog- www.reactivemetals.com

Hoover & Strong has a complete line of reticulated metals available.
We carry a full line of gold in colors and karat content that can be
ordered already reticulated or post reticulated. You can contact me,
or see our website HooverandStrong.com.

Steve Burns
National Account Manager
800-733-2642

I noticed that Hoover and Strong now offers reticulated sheets as
well as pre-depletion gilded sheets ready for reticulation.

Rudy Bescherer, Jr.

    I noticed that Hoover and Strong now offers reticulated sheets
as well as pre-depletion gilded sheets ready for reticulation. 

The interesting question here is: Has anybody used these products?
How do they work? Bill