Back to Ganoksin | FAQ | Contact

[Source] Platinum tubing


#1

Recently, platinum tubing has become scarce. I’ve exhausted the
following sources, all of whom no longer supply it:

Stuller
David H Fell
Precious Metals West
Hoover and Strong
Hauser and Miller
JC Nordt

Thanks for any info!
Lisa Krikawa


#2

Lisa- I can understand your frustration. If you can’t find a source
I’ll be happy to show you how to make seamless platinum tubing.

Have fun and make lots of jewelry.
Jo Haemer
timothywgreen.com


#3
Recently, platinum tubing has become scarce. 

You may have to make it.

James Binnion
James Binnion Metal Arts


#4

Yes, we have been looking as well-- and the same for palladium
tubing. No luck at all.

Noel


#5

I called Hoover and Strong and forwarded them the post about not
being able to source platinum tubing. They confirmed that they do
indeed still supply platinum tubing. They did reduce the number of
sizes available several years ago, but they do still make several
options.

Carol


#6

Hello James

Please can you show me how you will do a seamless tubing?

thks best
Adrien