Back to Ganoksin | FAQ | Contact

[Source] Niello

Hello,

I am looking for someone/some company which sells niello. USA -
Europe, it is not important. If you know someone, please let me
know.

Kindly,
Jacques Pinaud

Contact J. Loose
http://www.ganoksin.com/gnkurl/ep7z8g
He made some for me earlier this year.

Ric Furrer
doorcountyforgeworks.com

Karl Fischer, in Germany, sells it in bags of 100 gm.
http://www.ganoksin.com/gnkurl/ep7z8k

Elliot