Back to Ganoksin | FAQ | Contact

[Source] moissanite

Who knows how I can get some samples of the new diamond simulant
being marketed as moissanite???

Who knows how I can get some samples of the new diamond simulant
being marketed as moissanite???

From what I have heard moissanite will not be available for
about 4 more months.

Who knows how I can get some samples of the new diamond simulant
being marketed as moissanite???

The company that handles the moissanite is called C3 company,
Jeff hunter is the pres. They are based out of Raliegh North
Carolina. The phone number is 1-919-468-0399. I had the chance to
view the stones in Febuary 1997, and they tested possitive on the
regular diamond tester. The stones are off in color, I would say
L thru N. The stones that we looked at were under a carat. Maybe
size counts??? I was told that they have a tester for the stones
and that it was not ready yet. The price was around $ 300.00 a
carat Tammie

Hi Tammie: Thanks for the info on Moissanite , when you said They
have a diamond tester that is not ready, is it the producer of
the mossanite or another company? thanks chris