I know that everyone is heading to Tucson, but as I’m in a bind, I
thought I would give to forum a shot.

I need to find a source of.013 gauge 14kt gold wire or even finer
that can ship immediately. Unfortunately, I’m out of stock & Stearn
Leach always takes 3-6 weeks to fill my orders. I’d hate to pass up a
decent-sized sale because I’m out of stock on of one component…

As always, any suggestions would be much appreciated.


#2

Hi Jeet,

I need to find a source of.013 gauge 14kt gold wire or even finer
that can ship immediately. 

You might try Hauser and Miller (hauserandmiller.com), 800-462-7447
in St Louis…013 diameter wire is between 28 ga (.012") & 26 ga
(.014"). I’ve gotten 30 ga (.010") from them with no problems.

Usual disclaimers, just a satisfied customer.

Dave


#3

try hoover and strong in richmond va.


#4

Hi Jeet,

You can purchase this wire at Rio Grande. “Gem and Findings” catalog
– page 24 – item #604-128 Their phone number is: 800-545-6566 They
have all different ways to ship items to you. Dean Gordon

GOLDesigner Ltd.
Gold casting svcs.
http://www.goldesigner.com