Soldering silver to reticulated gold

Hello, I’m new to Orchid and I’m hoping you can help me out.

I would like to know if any of you know how to solder a reticulated
gold outer piece to an inner silver non-reticulated piece. It will
be used for a ring. After the soldering, I would like to edge the
top and bottom with a thick gold edging wire.

I would also like to embellish this ring with a bezel set stone.
Thank you for any help you may give.