I will use binding wire or soldering clay 

Jim, What is soldering clay?
Beth

The soldering clay is called Thermo-Fix Soldering Clay it is a some
what reusable water based clay that you can use to fixture pieces
when soldering it is sold by Frei& Borel

Jim