Soft soldering on chrome?

Has any one ever tried to soft solder (lead) onto chrome? Will
the chrome plating take the heat or will it discolor? And will
the solder bond to it?

I used to solder a lot of emblems to Zippo and other lighters.
We would grind off a patch of the chrome and tin solder to the
brass underneath.