Soft flex

soft flex also has a web site, at http://www.softflextm.com

i have been getting my artistic wire from them, some in exchange for
samples made up to show folks how it works up. i was amazed that the
"gold" colored copper wire wears as well as it does. i made a
bracelet and wore it for 2 1/2 months and it never turned my wrist
green, or the color chipped off. i am working up a line of samples
with the gold colored wire, but keeping it apart from my 14K gold
fill round wire. being slightly color blind doens’t help alot
either…

they also have a catalogue…

pat