Small nickel plating operation

I am looking for to set up a small nickel plating
operation. I work in stain glass and want to be able to plate
small and large pieces.

Thanks
Ted Hunt

A place to find plating supplies to do stained glass work is
from Dalmar, 11759 S. Cleveland Ave Suite 28, Fort Myers, FL
33907, 941-275-6540. E-mail dalmar@peganet. com They have a
Home Page http://www.peganet.com/dalmar/dalmarhm.html Just a
hint, Your lead must be completely free from all flux residue
and must first be plated in a cyanide based copper plate before
you can nickel plate. If this is not done first the nickel plate
will melt the lead.