Hey all!!

Has anyone on this forum had problems with sheet silver from Hardy and
Harmon?? I am having a problem with pits from impurities that show up as I
am buffing pieces. Also, the same silver does not take on a very good
polish. The finish can go from milky to looking like fine microscratches
have appeared on the piece (yes I used new buffing wheels) even with Zam and
red Rogue. The problem is intermittent, one bad batch between several good
batches.

If you are having a problem with your silver, I urge you to contact your
distributor and have them put pressure on Handy to upgrade thier quality
control processes.

Harry Butterfield
HP Trading Co.


#2

Yes and some of the fine bezzle will blow small bubbles. Lloyd