Rubber coating on stainless steel

Hi Dear Friends,

This time I have a question about " PU/Rubber Coating on Stainless
Steel". We use some domestic (China) paint on the stainless steel,
but it’s easy to peel off, even though use a nail to scratch it. ( We
found MONTBLANC have some jewelry with PU coating, and the coating is
very resistant). Is there anyone could teach me how to solve this
problem?

Thanks a million!
Waiting for your good news.

Frank
China

Hi Frank. How about Plasti Dip, a rubber coating for tool handles,
etc. It’s available in different colors from Home Depot and the
like. I’ve used it in several ways not intended by the manufacturer.

Allan