Jonathon, Belicone blue is not a zero shrink rubber. Most silicone
RTV is zero shrink, as is 4X ZeroShrink. Our silicone RTV can be
cured at room temperature in 16 hours, or in one hour at elevated
temperature. 4X ZeroShrink is a heat cure silicone rubber that does
not require special temperatures and resetting of vulcanizers in
order to achieve zero shrink.

4X ZeroShrink is an MJSA Innovation Award winner for 2007.