I was wondering if anyone knew where I gould buy shetts of silver/copper reticulation alloy? Isaac Coblentz
you can buy the alloy from Hoover and Strong 800-616-9997 or Hauser and Miller at 800-462-7447.
Elizabeth
Hoover and Strong 10700 Trade Road Richmond, VA 23236 1-800-759-9997
They make a special 80% silver 20% copper alloy for reticulation.
Rick Hamilton Richard D Hamilton, Jr. @rick_hamilton
I usually just make my own by making an alloy of 70% silver and running it through a rolling mill. Otherwise you might try to see if a refinery will do it for you. Also you might check Rio Grande. Tim Goodwin @tmn8tr