Back to Ganoksin | FAQ | Contact

Resin Burnout problem

Not all silicone RTV products are the same. Our Akron Silicone RTV
has been thoroughly tested with the viper resin and works just fine.
It may be that tin cure silicones react with the Viper resin.

If you are uncertain about your favorite silicone RTV, paint just a
little mixed RTV on a discarded Viper piece. If it does not cure,
you have your answer.

Good luck,

Bill Mull

Zero-D Products, Inc.
38285 North Lane. #103
Willoughby, OH 44094 USA
800-382-3271
440-942-1150
fax 440 942 2130
WWW.ZERODPRODUCTS.COM