Karen, I do a lot of beadwork which means very detailed silver to be
cleaned. The best and easiest stuff I ever used is Simple Green.
Just add Simple Green to cold water and let it soak for a few
minutes. Rinse and it’s clean. Does not harm pearls and stones, or
my hands. Great stuff!

Actually this was one of the first tips I learned at Orchid! Thank
you!

By the way, is it wise to tumble finished beaded jewelry? And what
is the best type of tumbler and process? I’m hopping for unexpensive
too…