I got so sick of the brown scum, even from a new can of Sparex, I
said Enough is enough, especially at the price. I went to my local
swimming pool supplies dealer and bought a canister of sodium
bisulfate(sp?) and have been using it ever since. Much cheaper and
produces an extremely clean product. I cannot see why anyone would
continue to use Sparex. John Barton