Pure copper chain

Hello Bobby,

Instead of copper, how about using fabric cords (like linen) or
leather. Copper chain has a bad habit of leaving green marks on
skin, which is not customer friendly - usually people are not
pleased.

Judy in Kansas, where the rains have been falling for several days.
Hardly allows time for the lawn to dry enough so that it can be
mowed.