Peter and others: thought I’d add this as I usually do in Pripps
posts. TSP in alot of states is hard to get because its
environmentally unfriendly. The stuff labeled TSP in hardware
stores, if you read the fine print is something else. However you
can find REAL TSP at any beer brewing supply place, its what they
use for cleaning beer bottles before bottling. The other stuff
makes a messy solution thats really gummy and doens’t work so
well. Dave