I would like to append the original message-it made sense when I
wrote it, but I guess I was a little sleepy! I am looking for a
manufacturer who will sell me tags with my logo neatly pre- stamped on
it. They are in the same size and shape as the ones in Rio catalogue
but I’ve seen them come on a sheet and you pop them off and file the
edge where it attached and presto!. I think they might be
photo-etched or machine stamped. I’m not lazy, just way too busy to
bang them out myself and I need quantity in Sterling and karat gold.
(Thank you all who took the time to recommend Rio Grand though) Does
this help anyone who might be able to help me? I am still new at this
so I thank you in advance for your patience as I am still wobbly with
the lingo- (Also I am not looking for someone to do this by hand-the
logo is very detailed.) whew Meike
Meike,
Have you contacted MJSA (Manufacturing Jewelers and Supplies of
America) and asked them for a referral? They may be able to give you
the names of a member or members that provide this type of product.
You can try the online search function, ReferralNet, at
http://www.mjsainc.com, but for something this detailed, I’d suggest
calling and talking to a member service representative at (800)
444-6572.
You don’t have to be a member of MJSA to request a referral or ask
for their assistance tracking down a product. However, you do have to
be a member to have callers referred to you, so if you’re a supplier
or manufacturer, you might want to consider joining so that the
association can refer potential clients to you. ![]()
Suzanne
Suzanne Wade
AJM Contributing Editor
Suzanne@rswade.net
Phone: (508) 339-7366
Fax: (520) 563-8255
Meike, I would recommend Arch Crown. They have many labels and
services available for tags and labels. http://www.archcrown.com/
800.526.8353
Hope this helps! Rebecca.