I’ve used Chromium Oxide for a number of years to polish mostly
green nephrite jade which I think I purchased through Diamond
Pacific Corp. in California. It’s a green very fine powder (which I
use only with thin plastic gloves running between wet and dry.) Feel
free to email me personally for further details. Jot Singh Khalsa