Polishing cabs


#1

One test that I have used in the past is to polish half of the cab
on diamond and the other half on compound, then check the
difference. Diamond is an abrading process and sometimes does not do
the greatest job. Other times is it fast, clean and bright. Like
some of the postings have said: There is no magic powder.