Back to Ganoksin | FAQ | Contact

Pickling Station Set Up

Hello all,

Does anyone have any tips for setting up a pickle pot station with ventilation? Or even better, specific plans for how to set one up? What I’m looking for is what kind of fan to use to place in that window, plans of the ducting, attaching the ducting, etc. Alternatively, what do people think about ductless extraction hoods? Expensive, yes, but also means I won’t be giving up a window and won’t be dealing with temperature issues in the studio.

Pictures of people’s home builds would be deeply appreciated. I’m a visual learner - as are most of us here, I’m sure!

Thanks for the help!