The alloy which is mainly sold in Germany is 50% Ag and Pd each. It
is darker than platinum, soft zu work with, it has a nice steel like
colour and you can melt fine gold or silver on it without being
altered the base metal. You can also use 33% Pd and 67% Ag which is a
bit darker even. Great metal and not costly! You can cast it in the
Dutch Delft sand, also sheet and wire for all further purposes. Great
stuff!