Hi Y’all,

Does anyone on this list own an MPulse Orion PUK welder? I have had
mine for about 3 months and still have many questions, particularly
about welding sterling silver (it’s very mobile and tough to
control.)

Looking for some wisdom and possible tricks to employ.

Thanks in advance.