Back to Ganoksin | FAQ | Contact

Organic stamp tools


#1

Hello, I hope someone can help me…

I am looking for stamping tools with organic looking stamps such as
cherry blossoms, lotus flowers, or chinese lettering, does anyone
know where to find these?

I am also looking for a source for rose gold filled sheet and chain,

Any help would be great.

Thanks
Bari


#2

Hi Bari

I am looking for stamping tools with organic looking stamps such
as cherry blossoms, lotus flowers, or chinese lettering, does
anyone know where to find these? 

I couldn’t dig out the catalog to double-check (it’s packed away
temporarily), but you could check Indian Jeweler’s Supply. If I
remember right, they have a very large collection of stamps.

Good Luck
Kim Starbard


#3

Also, if you have an image you would like made into a stamp,
Microstamp Corp can do that for you.

http://www.microstampusa.com/

Linda