I'm with you Brian, I never work-harden posts, they harden even in
the mild wear and tear of showing the earrings to customers. Lisa
(its stopped raining!) in Topanga,CA

Perverse aren’t we? It’s important to recognise that work
hardening is a continuum not a perfect state, and eventually
they’ll get fatigued (is that too strong?).

Brian - winter is astirring. Well we had a nice summer.
B r i a n =A0 A d a m J e w e l l e r y E y e w e a r =A0
@Brian_Adam1 ph/fx +64 9 817 6816 NEW ZEALAND