Hey, what is this Omega stuff I keep hearing about? Is it a jewelry
manufacturer or a designer? I saw some pieces at the jewerly store where I
buy stones etc. and wonder what all the fuss is about? Dave

Art Jewelry for Conscious People
http://www.opendoor.com/stephensdesign/crystalguy.html


#2

Are you referring to Omega (armor) style necklaces/bracelets?? The
least durable chain design around.
Ringold’s Jewelers since 1908 9865 Bustleton Ave/ Phila, PA 19115
215-671-8190 Fax: 215-969-1803 Ringold@IX.netcom.com
Http://home.aol.com/REGALITE
Manufacturing / Mining / Product Development


#3

Dave Stephens wrote:

Hey, what is this Omega stuff I keep hearing about? Is it a jewelry
manufacturer or a designer? I saw some pieces at the jewerly store where I
buy stones etc. and wonder what all the fuss is about? Dave

Dave - Omega is a manufacturer of fine gold chains - very thick and
luxurious, flat on the back and domed on the front. Please note that if
you are given one to solder or repair that there are tiny steel cables
running through the inside. This is the primary chain for which most
"slide" pendants are designed. Mike