Casdaldo No Shrink Pink does shrink. With careful measurements, using
no model in the mold frame (solid filled mold frame), the best result
I could get was 1.2%. I arrived at this by measuring the mold and
mold frame opening using an optical comparator. If you want
a Non-Shrinking Mold, use a Silicone RTV. Craig Miller