Nitric Acid Disposal Dilemma

Christel,

STOP, do not place Nitric Acid in a metal sink. I am not sure whether
or not your idea of placing this bottle in a water filled tank will
work or not but Nitric Acid and Steel is not a good combination.

Greg DeMark
www.demarkjewelry.com